TZP-ZrO2 and ZTA- performance parameters
发布时间:2014-11-30 点击量:
Table 3:TZP-ZrO2和ZTA-Zirconia toughened alumina ceramics performance parameters |
Item |
Test conditions and units |
3y-TZP
氧化锆瓷
|
8y-TZP
氧化锆瓷
|
ZTA
25%ZrO2
|
ZTA
25%ZrO2
|
Static bending strength |
室温Mpa |
1100 |
300 |
700 |
800 |
Fracture Toughness |
Mpa·m |
≥7 |
≥1.5 |
≥5 |
≥5.5 |
Hardness |
HRc |
≥9.00 |
≥9.00 |
≥9.02 |
≥9.02 |
Elastic Modulus |
Gpa |
200 |
50 |
250 |
250 |
Bulk density |
g/cm3 |
≥6.0 |
≥6.0 |
≥4.5 |
≥4.8 |
Coefficient of thermal expansion |
200ºC×10-6/ºC |
10 |
10 |
9.2 |
8.5 |
Heat drawability |
ºC |
250 |
250 |
450 |
450 |
Water absorption |
% |
0 |
0 |
0 |
0 |
|